During hot extrusion, the casting rod must be heated to make the metal have higher plasticity, reduce deformation resistance, and create conditions for the profile to obtain better mechanical properties during aging.To get a higher intensity.Higher extrusion temperature should be selected, but good surface quality must be ensured.Generally, the casting rod temperature is controlled between 440 ℃ and 500℃.Electrical modular enclosure perfect details :
Whether the heat sink: | Heat sink |
Material: | AL6063 T5 |
Application: | Inverter router ect element products |
Tensile strength: | sigma b (MPa) ≥205 |